Main Metall – CoCr alloy for high demands
Indications
– Wide span ceramic veneered restorations
– Implant retained restorations
– Combinated restorations
Typical values
yield strength RP 0,2 % (MPa) | 570 |
elongation (%) | 4,2 |
young’s modul (GPa) | 190 |
tensile strength (MPa) | 725 |
density (g/cm3) | 8,7 |
casting temperature (°C) | 1474 |
WAK CTE (25 – 500°C) |
14,0 |
hardness (HV 10/30) | 370 |
dimensions (mm) | Ø 8 x 15 |
type acc. DIN EN ISO 22674 | ≥ Type 5 as delivered |
Lot numbers may show minimum deviation from typical values.
More information are available on our instruction for use.
Chemical Composition
Co | Cr | W | Nb | Mo | Si | V | Others |
60,2 | 25,25 | 9 | 2,2 | 1,05 | 1 | 1 | < 0,1 |