KERA® S-POWDER – CoCr powder for laser-sintering
Approved for the most usual laser-sintering systems
Indications
– Ceramic veneered crowns and bridges
– Tertiary structures
Typical values
yield strength RP 0,2 % (MPa) | 375 |
elongation (%) | 14,7 |
young’s modul (GPa) | 240 |
tensile strength (MPa) | 525 |
density (g/cm3) | 8,55 |
WAK CTE (25 – 500°C) |
14,5 |
hardness (HV 10/30) | 285* |
Grain Size | 10 – 45 μm (±5%) |
type acc. DIN EN ISO 22674 | ≥ Type 4 as delivered |
Lot numbers may show minimum deviation from typical values.
More information are available on our instruction for use.
Chemical Composition
Co | Cr | W | Si | Mn | Fe | Others |
61,65 | 27,75 | 8,45 | 1,61 | 0,25 | 0,2 | < 0,1 |